Ce este echivalentul ASTM A790?

May 26, 2025

Lăsaţi un mesaj

 

Ce este ASTM A790?

ASTM A790 is a standard specification for seamless and welded ferritic/austenitic stainless steel pipe, also known as duplex stainless steel pipe. It is primarily used in applications requiring high strength, excellent corrosion resistance, and good weldability, such as chemical processing, oil and gas, and marine environments.

 

Ce este echivalentul ASTM A790?

Gradul ASTM A790 Desemnarea UNS Ro / Din echivalent Nume comun
A790 S31803 / S32205 UNS S31803 / S32205 Ro 1.4462 / x2crnimon 22-5-3 Duplex 2205
A790 S32750 UNS S32750 Ro 1.4410 / x2crnimon 25-7-4 Super Duplex 2507
A790 S32760 UNS S32760 Ro 1.4501 / x2crnimocuwn 25-7-4 Super duplex (Zeron 100)
A790 S32304 UNS S32304 Ro 1.4362 / x2crnin 23-4 Lean Duplex 2304

 

ASTM A790 Compoziție chimică

 ASTM A790 Chemical Composition

Proprietăți mecanice ASTM A790

ASTM A790 Mechanical Properties

 

Ce material este ASTM A790 UNS S31803?

ASTM A890 CD3Mn or Grade 4A is the nearest equivalent grade to the wrought super duplex stainless steel UNS S32205. It is also designated as ASTM A995 and ASME SA351/995 grade CD3Mn or 4A, also written as J92205 or X2CrNiMoN22.


Ce este materialul ASTM A790 UNS S32760?

Astm A790 Uns S32760 Welded Pipes have a smooth finish as they are made from cold-formed stainless steel and also have strong mechanical traits. They are resistant to chloride pitting and coercive corrosion. 18 Swg., 14 20 Swg., Swg . swg ., 12 16 swg ., 10 swg .

 

Care este diferența dintre S31803 și S32205?

S32205 are un control mai strâns al compoziției și o rezistență la coroziune îmbunătățită în comparație cu S 31803.

 